Physical Properties | Unit | Test Method |
Machine Wrap Film |
Hand Wrap Film |
Hand Wrap Film |
---|---|---|---|---|---|
Thickness | u | -- | 20 | 20 | 20 |
Specific Gravity | -- | ASTM D 1505 | 0.916 | 0.916 | 0.916 |
Tensile Strength At Break | MD/CD kg/cm² | ASTM D882 | 240 | 250 | 240 |
180 | 190 | 180 | |||
Elongation At Break | MD/CD % | ASTM D882 | 420 | 430 | 420 |
690 | 580 | 580 | |||
Tear Strength | MD/CD g | ASTM D 1922 | 60 | 90 | 20 |
430 | 420 | 420 | |||
Haze | % | ASTM D 1003 | 1.7 | 1.6 | 1.6 |
Gloss 60 | % | ASTM D 2457 | 130 | 130 | 130 |